Development of Smelting Reduction Processes for Ironmaking satyendra March 8, 2017 0 Comments blast furnace, direct reuction, DR process, DRI, exhaust gas, Hot metal, melting, reduction, smelting reduction, SR processes, Read More
Corex Process for Production of Iron satyendra February 22, 2017 0 Comments Corex gas, Corex process, Dome, DRI, export gas, Hot metal, Iron ore lump, Melter-Gasifier, non coking coal, pellets, Reduction furnace, Read More
Coal based Direct Reduction Rotary Kiln Process satyendra February 14, 2017 2 Comments Boudouard reaction, dolomite, DRI, Iron ore, metallization, non coking coal, pellets, reduction, Rotary kiln, Sponge iron, Sulphur, Read More
Steel Scrap and Scrap Sorting and Preparation Processes satyendra January 23, 2017 6 Comments baling, Briquetting, detinning, dezincing, magnetic separation, scrap, scrap sorting, shearing, shredding, steel, Read More
Rolling of hot strip and strip defects satyendra January 14, 2017 0 Comments camber, elastic transformation, hot rolling, plastic transformation, roll pressure, rolling, rolling load, strip levelling, waviness, Read More
Automation in Steel Industry satyendra December 29, 2016 0 Comments automation, computers, controls, digital controller. automation levels, distribted controls, functional hierarchy, input/output, instruments, Programmable controllers, Read More
Processes for Forging of Metals satyendra December 16, 2016 0 Comments Bending, die, drawing, edging, flatting, forging, Hammer, Presses, pressing, Punching, Swaging, Read More
Processes for Casting of Metals satyendra December 7, 2016 0 Comments centrifugal casting, continuous casting, Die casting, expendable mould casting. Non expendable mould casting, Investment casting, permanent mould casting, Plaster mould csting, sand casting, Read More
Wire and Rod Drawing Process for Steel satyendra November 13, 2016 30 Comments carbon steel, dies, Ductility, lubrication, percent reduction, rods, rounds, stainless steel, wire drawing, wire rods, Yield strength, Read More
Metallurgical Principles in the Heat Treatment of Steels satyendra November 4, 2016 0 Comments annealing, austenite, carburizing, cementitem eutectic, eutectoid, Ferrite, graphite, heat treatment, nitriding, normalizing, quenching, tempering, Read More