Tinplate and Process of Tinning

Tinplate and Process of Tinning Tinning or tinplating is the process of thinly coating sheet or strip of steel with tin (Sn), and the resulting product is known as tinplate. Tinplate is light gauge, cold-reduced low-carbon steel sheet or strip, coated on both faces with commercially pure tin. It combines the strength and formability of steel and the corrosion resistance, …