Refractory Lining of Coreless Induction Furnace

Refractory Lining of Coreless Induction Furnace In steel melting shops of low capacities, induction furnace is preferred as a convenient melting unit because of its high efficiency, low energy consumption, easy operational control, and good performance with various kinds of steel scrap. The induction furnace is an electrical furnace in which the heat is applied …