Metallurgical Processes and Defects in Steel Products satyendra October 10, 2016 12 Comments camber, Flatness, inclusion, lamination, Overlap, Piping< Cracks, porosity, Seams, shape, Slivers, Tears, Wedge, Read More
Characteristics of Steel Wire Rods satyendra January 3, 2014 3 Comments cold heading, cracks, electrode quality, Fins, high carbon, Laps, Scabs, Slivers, wire rod coils, wire rod mill, wire rods, Read More