Glossary of technical terms for the use of metallurgical engineers Terms starting with alphabet ‘H’

Glossary of technical terms for the use of metallurgical engineers Terms starting with alphabet ‘H’ H-13 tool steel – It is a chromium-molybdenum-vanadium hot-work tool steel, widely considered the ‘workhorse’ of the tooling industry. It is defined by high toughness, excellent resistance to thermal fatigue (heat checking), and superior wear resistance. H-13 tool steel is predominantly …